  • This premixed powder uses Cast Tungsten Carbide (CTC) powder as hardphase to blend with and nickel-based self-fluxing alloy. CTC is irregular with high hardness (≥ 1) and excellent wear resistance. Nickel-based alloy powder is spherical or near-spherical and has excellent wettability with cast tungsten carbide. The premixed powders with different CTC contents and particles are suitable for PTA (Plasma Transferred Arc) welding, LC (Laser Cladding), and FS (Flame spray).
  • The welding overlay has excellent wear resistance with low porosity.
  • Mainly used in wear resistance, anti-abrasion surface or wear repair for mining extraction, oil drilling, machinery equipment, and oil equipment.

Components

Grade

Hardphase

Bonding-phase

ZTC68

MTC

Nickel-based alloy powder

*: We can tailor-make different particle sizes, Nickel-based alloys, and CTC contents for various applications.

Typical Grades

Grade

Composition (Wt, %)

Size

(µm)

Size

(mesh)

Overlay Hardness (HRC)

MTC

Nikel-based Powder

ZTC683344

40

60

150 + 45

100 + 325

50 56

ZTC683345

50

50

150 + 45

100 + 325

52 56

ZTC683346

60

40

150 + 45

100 + 325

52 58