WC-20Cr3C2-7Ni hitauppstreymisduft

  • Agglomerated and sintered gray-black spherical or near-spherical particles with good flowability.
  • The maximum service temperature is up to 750℃. It can be used in humid environments.
  • The dense coating has excellent resistance to oxidation, corrosion, and abrasion.
  • Anti-oxidation and corrosion resistance are better than WC-Co – based coatings.
  • Mainly used in the steel & iron industry, paper making, pump valves, etc.

Einkunn og efnasamsetning

Einkunn

Efnasamsetning (Wt, %)

W

T. C 

Ni

Kr

Fe

O

ZTC48D*

Jafnvægi

5.8 – 6.4

6 – 8

20 – 23

≤ 0,5

≤ 0,5

*: D stands for spherical or nearly spherical thermal spray powder.

Stærð og eðlisfræðilegir eiginleikar

Einkunn

Gerð

Stærðarbrot (μm)

Sýnilegur þéttleiki (g/cm³)

Rennslishraði

(s/50g)

Umsókn

ZTC4851D

WC – Cr3C2 – Ni

73/20/7 Agglomerated

& Sinterað

– 53 + 20

≥ 4

≤ 18

  • HVOF

(JP5000 & JP8000, DJ2600 & DJ2700, JetKote,

Woka Jet, K2)

  • HVAF
  • APS

ZTC4853D

– 45 + 20

≥ 4

≤ 18

ZTC4852D

– 45 + 15

≥ 4

≤ 18

ZTC4881D

– 45 + 11

≥ 4

≤ 18

ZTC4854D

– 38 + 10

≥ 4

≤ 18

ZTC4882D

– 30 + 10

≥ 4

≤ 30

Við getum sérsniðið mismunandi kornastærðardreifingu og augljósan þéttleika fyrir ýmis forrit.
Ráðlagðar úðafæribreytur (HVOF)

Húðunareiginleikar

Efni

WC -20Cr3C2 – 7Ni

hörku (HV0.3)

950 – 1200

Framleiðsla

Sambyggð & Sintered

Tengistyrkur (MPa)

> 70MPa

Stærðarbrot ( µm )

– 45 + 15

Innborguð skilvirkni (%)

35 – 45%

Spray Torch

JP5000

Porosity (%)

< 1%

Stútur (tommu)

6

Steinolía (L/klst.)

23

Súrefni (l/mín.)

900

Flutningsgas (Ar) (L/mín.)

8.0

Fóðurhraði dufts (g/mín.)

70 – 80

Sprautufjarlægð (mm)

340 – 360